Coating defects caused by improper use of atomic ash


 Coating defects caused by improper use of atomic ash

 
In the automobile coating process, the top coat is the last process of Z. with the continuous development of the automobile industry, many manufacturers now use baking paint. If there is a problem after finishing, it is Z troublesome. The following atomic ash manufacturers will make a brief introduction according to the problems in production.
 
1. The top coat foams after baking.
 
Scrape off the bubbles after the bubbles of the top coat and see which layer the bubbles are on. If the bubbles appear in the primer layer, the atomic ash is well combined with the primer, and the substrate treatment may not be in place; After blowing off the bubbles, it is found that there is a layer of primer on the atomic ash and the substrate. Then it may be that the primer is too thick or the primer is not dry enough.
 
2. Pinholes and depressions appear after baking the finish paint.
 
First of all, consider whether the pinhole has its own quality. Secondly, if pinholes appear when the quality of atomic ash is qualified, it is generally because the atomic ash coating and grinding technology is poor and the sand holes are not handled well. In addition, during the coating and scraping process, if the coating and scraping tool is improperly selected, it will also cause pinholes.
 
3. "Prickle" after baking the finish coat.
 
First, the climate is too humid and the water absorption of the atomic ash is too large. The polished atomic ash adsorbs a considerable amount of water. The topcoat is sprayed before the water volatilizes. A small amount of water is sealed under the paint film. Once heated, the water volume expands sharply and breaks through the paint film to form a "prickly heat". Second, the water absorption of atomic ash is qualified. After being dried by hot air, spray the top coat, and there is "prickly heat" after baking. Then it is possible that after spraying the top coat, the solvent enters the drying room before it volatilizes fully. In this way, because the surface of the top coat is closed soon, the residual solvent has to break through the paint film to form "prickly heat". Of course, it may also be the quality problem of the topcoat, or the mismatch between the polarity of the solvent and the topcoat


Prev What are the types of atomic ash
NextSteps for scraping atomic ash

Copyright © 2020 Changxing Baodi Environmental Protection Technology Co., Ltd all reserved Web Admin --> >>

浙公網安備 33052202000243號?浙ICP備17019658號

主站蜘蛛池模板: 精品久久久久久亚洲精品 | 久久久久久久久久久影视 | 一区二区三视频 | 国产精品7区 | 国产一区二区三区四区波多野结衣 | 久久国产一二三 | 性欧美性欧美 | 精品国产一区二区三区成人影院 | h视频在线免费观看 | 欧美日韩色片 | 91麻豆精品国产91久久久更新资源速度超快 | 亚洲综人网| 九九热在线视频免费观看 | 日韩精品久久久久久久电影99爱 | 91久久线看在观草草青青 | 欧美大片一级毛片 | 一级α片| 羞羞的动漫在线观看 | www.48xx.com| 国产精品麻豆一区二区三区 | 青青草好吊色 | 国产精品一区网站 | 成人毛片视频在线观看 | 欧美视频在线一区二区三区 | 国产成视频在线观看 | 九九热精品在线 | 最新毛片在线观看 | 久久国产精品无码网站 | 久久久久久久久久亚洲精品 | 黄色免费av| 毛片视频网站 | 午夜视频福利 | 欧美激情精品久久久久久久久久 | 国产噜噜噜噜久久久久久久久 | 97青青 | 欧美a级在线免费观看 | 久草在线资源福利站 | 在线a毛片免费视频观看 | 二级大黄大片高清在线视频 | 激情久久精品 | 免费视频一区 |